Polyester Backing Fabric factory talks about the setting of Polyester Backing Fabric
Polyester Backing Fabric factory considers Polyester Backing Fabric to be a material, waterproof oxford is mainly a way of weaving, possibly with polyester fabric. Polyester Backing Fabric is a kind of raw material, there are hundreds of thousands of specifications and models, waterproof Oxford cloth is one of them.
1. Polyester Backing Fabric setting temperature: 170℃—200℃, speed: 20M—28M/min.
2. The color of the Polyester Backing Fabric factory generally does not change much, but the sublimation fastness of the red dye is not good. After finishing, the chassis will leave dyes. It cannot be made light color immediately, only black can be used, and more waste cloth can be used. Second machine, can do light color.
3. The Polyester Backing Fabric factory has a large shrinkage rate of polyester pull frame cloth. If the customer requires good elasticity, small shrinkage rate and good hand feel, the embryonic cloth must be pre-determined and dead. Pay special attention to black and white, red and white flowers, because the dye sublimation fastness is not good, the finished product Styling must be low temperature, such as high temperature will seriously stick to the product.
4. Polyester Backing Fabric factory polyester bobbin fabric setting, pay attention to the thickness of the middle and edge of the fabric, the temperature should be well controlled, not too high, the speed of the machine should be slow, and it should be pulled in two times. The difference between the thickness of the middle and the edge can be reduced by two determinations. For the first determination, the width of the door is about 6-8 inches less than the finished product, and the weight is about 100 grams. The temperature of the second time is 5-10 degrees lower than that of the first time, and the width and weight of the door are as required.